This tester is used to test the characters of film

Standards:

ISO 7765-85, ASTM D 1709 and the equivalent.

Parameters:

◆ Impact energy: 30J.

◆ Impact height: Method A is 660mm and Method B is 1500mm.

◆ Diameter of dart head: d=38mm±1 mm in Method A, d=50mm±1mm in Method B.

◆ Mass of the dart: 50g to 2000g, increasing by 5g.

◆ Mass accuracy of the dart: 0.5%.

◆ Inside diameter of the clamp: 125mm.

◆ Outside diameter of the clamp:150mm.